Finally got around to running these over the chronograph. 10 gr. Universal, dacron filler this time, NOE 165 SC311-165 RF, PC'd and water quenched, sized .3112, in Federal cases. Surprized me a little with an ave. of 1440 fps, ES 23, for 5 shots. Not as slow as I was guessing, but then those Fed cases are heavy.
I dug around and found a couple hundred 31141 GC left over from a 30-30 project over 15 years ago. They were water quenched out of the mold, gas checked, sized .3105 and coated with LLA. I've got a light coat of BLL drying now since the old coat of LLA was pretty dry. I'll play around with a couple loads for a higher velocity loading.
Does anyone have a preference between the original Lyman, the Accurate version, or the Noe version of the 311041? I know it will be easier to get the larger dia I need from either of the custom molds.