fiver Well-Known Member Apr 26, 2020 #21 lino would shear with noses like that. mono would probably break up into pieces once the shearing started.
lino would shear with noses like that. mono would probably break up into pieces once the shearing started.
CWLONGSHOT Well-Known Member Apr 27, 2020 #22 I cast them two alloys. 20:1 and 25% WW 75% soft alloy. I usually get about a 10BHN from this last mix. I sent a bunch off to my buddy who can shoot them into wet news print. One I kept are 20:1 and sized 356 to try in the lil 357 Sig. on coyotes. . We got one last week. But they are scarce I’m thinking pups still small so they mostly staying near dens. CW
I cast them two alloys. 20:1 and 25% WW 75% soft alloy. I usually get about a 10BHN from this last mix. I sent a bunch off to my buddy who can shoot them into wet news print. One I kept are 20:1 and sized 356 to try in the lil 357 Sig. on coyotes. . We got one last week. But they are scarce I’m thinking pups still small so they mostly staying near dens. CW