Ian
Notorious member
Mostly it's displaced vent line "whiskers" that get partially pulled out when the blocks are opened and then mashed back into the faces when the blocks are closed. Running the mould hot for complete fillout and using more than about 1% tin will exacerbate this with some moulds depending on how big the vent lines are and how blocked the vent lines are by the metal displaced by the cavity being machined.